Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purity Applications: - Chemical processing – production, storage and transfer of corrosive fluids
- Electronics – protective sheathing, plenum and wiring insulation
- Semi-conductor industry
- Food stuff and Healthcare industries
- Transportation – fuel line and pipe, thermoformed body components
Information provided by Arkema Inc. |