MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Synprene® RT-3810M Thermoplastic Elastomer - SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Description/Features:

  • High Performance Thermoplastic Elastomer
  • Natural

Applications:

  • Multi-Purpose
  • FDA (Food Contact)

Market:

  • Consumer Goods

Processing Method:

  • Injection Molding
PolyOne First Choice

Disclaimer: A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. This statement is only an overview of the FDA listings for this product. IT IS THE CUSTOMER'S RESPONSIBILITY TO ENSURE THAT THE COMPOUND IS SUITABLE FOR ITS INTENDED APPLICATIONS.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 10Instant; ASTM D2240
Tensile Strength at Break 275 psiMethod A (Dumbbell & Section), 20 in/min; ASTM D412
Tensile Stress at Strain 50.0 psi
@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 800 %Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 65 %Bayshore; ASTM D2632
Tear Strength 45.0 pliDie C (graves), 20 in/min; ASTM D624
Compression Set 30 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -85.0 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Overview of materials for Styrenic Elastomer (TES)
Overview of materials for Styrene-Butadiene Copolymer, SBC
Kraton® G1750X (EP)n Multi-Arm Copolymer
Avient Synprene® ST-6110 Thermoplastic Elastomer - SBC

PH1PO3260 / 44972

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.