HexPly® M47 is a toughened, self extinguishing 140ºC curing epoxy resin matrix that has been developed for the performance car market. It exhibits good strength retention at elevated temperature, good processability and excellent surface finish. Its high Tg allows HexPly® M47 to be considered as an alternative to 180ºC curing matrices when a lower curing temperature is required.Information provided by HexCel |