MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics IFB Insulation Range JM ™ 25 SL Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Temperature range: 1350-1650°C. Manufacturing method: slinger. The IFB range is manufactured via cast (K®) and slinger (JM™) processes, is a market leader in applications such as Petrochemical and Ceramics where the ability to operate in environments above 1000°C (1800°F) is critical. The range also provides low thermal conductivity due its unique manufacturing process. Our IFBs deliver energy savings for multiple markets and our global manufacturing footprint enables Morgan to meet your regional and global application demands.

Applications: Hot face refractory lining or as back-up insulation in:

  • Aluminium (anode bake furnaces, primary electrolytic cells, holding and melting furnaces and secondary re-melt furnaces)
  • Petrochemical (kilns, flues, refining vessels and heaters and reactor chambers)
  • Iron and steel industry (heat treatment and galvanising)
  • Coke and iron making (blast furnaces, hot blast stoves, hot blast and bustle main)
  • Hobby and laboratory kilns
  • Ceramic industry (including kilns for domestic use)
  • Lime and cement kilns
  • Glass industry

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.720 g/ccASTM C-133
Deformation 2.0 %
@Temperature 1200 °C,
Time 5400 sec
0.069 MPa; ASTM C-16
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00100 GPaASTM C-133
Compressive Strength 1.30 MPaCold Crushing Strength; ASTM C-133
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.260 BTU/lb-°FASTM C-182
Thermal Conductivity 0.220 W/m-K
@Temperature 400 °C
ASTM C-182
 0.250 W/m-K
@Temperature 600 °C
ASTM C-182
 0.290 W/m-K
@Temperature 800 °C
ASTM C-182
 0.340 W/m-K
@Temperature 1000 °C
ASTM C-182
Shrinkage 0.50 %
@Treatment Temp. 1290 °C,
Time 86400 sec
ASTM C-210
 
Component Elements PropertiesOriginal ValueComments
Al2O3 48 %
CaO 0.10 %
Fe2O3 0.90 %
Other 1.9 %MgO + Na2O + K2O
SiO2 47 %
TiO2 0.50 %
 
Descriptive Properties
Classification Temperature (°C)1350
Reversible Linear Expansion (%)0.55

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6188 / 202972

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.