MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Oil Rust Proof
Categories: Fluid; Lubricant

Material Notes: Texaco Rust Proof Oil delivers value through:
  • Good short-term rust protection — Low viscosity oil provides complete coverage of metal surfaces for maximum protection against oxidation and corrosion. After evaporation of the solvent, a thin, highly protective, nondrying oily film remains to protect the metal. Oxidation and corrosion inhibitors in the oil resist chemical attack by air, water, other fluids and particulate matter.
  • Easy application and rapid run-off — Low viscosity assures easy application, complete coverage and fast drain-off of excess oil. High volatility of the solvent ensures rapid evaporation, minimizing post-application dripping.
  • Easy removal — Thin transparent oily film is readily soluble in petroleum solvent or kerosene to enable easy removal when required.

Texaco Rust Proof Oil is a low viscosity, rust protective oil designed for the temporary rust protection of steel in covered storage or packaged shipment.

It contains oxidation and corrosion inhibitors and is diluted with a petroleum solvent for ease of application.

Texaco Rust Proof Oil is recommended for use as temporary protection of sheet steel, hand tools, small parts, bearings and highly machined surfaces under relatively mild conditions of indoor storage, packaged shipment or inter-process handling.

May be applied by brush, dip or spray.

Where a higher level of oily film rust protection is required, Texaco Metal Protective Oil L should be used.

Where rusting conditions are severe, Texaco Rust Proof Compound is recommended.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220564; MSDS Number: 10663

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 38.5 °
Saybolt Viscosity at 100°F 40 SUS
Kinematic Viscosity at 40°C (104°F) 3.5 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °C
Flash Point 54.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ecoflex® F BX 7011 Biodegradable Plastic
Overview of materials for Low Alloy Steel
Overview of materials for High Carbon Steel
Overview of materials for Cold Work Steel
Overview of materials for AISI 4000 Series Steel

WTEXA173 / 77052

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.