MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kohesi Bond KB 1041 AL Two component epoxy for bonding, sealing, coating and potting applications
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Thermally Conductive

Material Notes: Product Highlights:
  • Superior thermal conductivity > 4.5 W/m/K
  • Excellent chemical resistance
  • Superb mechanical strength properties
  • Good flow properties
  • Easy to use mix ratio of 100:10 by weight
  • Very good dimensional stability
Kohesi Bond KB 1041 AL is a two component, room temperature curing epoxy system suitable for bonding, sealing, potting and encapsulation. It has a favorable 100:10 (Part A: Part B) mix ratio by weight. This epoxy system offers excellent adhesion to a variety of substrates, such as metals, glass, ceramics, most plastics and rubbers. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1040 offers first-rate thermal conductivity (> 4.5 W/m/K), ideal for heat sink bonding. It has a smooth glossy appearance upon cure. It offers an extensive service temperature range of -50°C to +150°C. This adhesive fosters outstanding mechanical strength properties, especially under tensile and compression. It offers minimal shrinkage upon cure and cures rigid. In addition to a long working life, it also offers good chemical resistance to a variety of fuels, oils, acids, bases and boiling water. Part A is gray in color and Part B light yellow - clear in color. KB 1041 AL is widely used in optical, aerospace, electronics, specialty OEM and related industries.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 10 - 250 cPPart B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 70
Tensile Strength >= 8000 psi
Tensile Modulus >= 350000 psi
Adhesive Bond Strength >= 2500 psiTensile Lap Shear, Al/Al
Peel Strength 20.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 25.0 µm/m-°C
Thermal Conductivity >= 4.50 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 90.0 °C
Option 2
 3.00 - 5.00 hour
@Temperature 70.0 - 90.0 °C
Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
 48.0 - 72.0 hour
@Temperature 23.0 °C
Option 1
Working Life >= 70.0 min100 g of mixed epoxy
Shelf Life 6.00 Monthin original unopened containers
 
Descriptive Properties
Mixing Ratio100:10 by weightPart A : Part B
ViscosityThixotropic PastePart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOHESI922 / 249101

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.