MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM PR/04 AFKN NERO UP Thermoplastic Compound
Categories: Polymer; Thermoset

Material Notes: FRAGOM: It is our thermoplastic compound with low flame propagation under fire conditions. The material is low smoke, halogen free and heavy-metal free.

FRAGOM PR/04 AFKN NERO UP: is designed to extrude cable sheathing at high speed without any migration risks as it is completely free of plasticizers. This grade contains >2.5% wt of carbon black and suitable UV stabilizers for outdoor applications. Suitable for sheathing extrusion of cables with size <60 mm2.

Certify: CEI 2011 M1, VDE 0207 HM2-HM4, BS7655 LTS1-LTS2-LTS3-LTS4

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Melt Flow 5.0 - 10 g/10 min
@Load 21.6 kg,
Temperature 160 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength >= 11.0 MPaIEC 60811
 >= 14.3 MPa
@Temperature 110 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Elongation at Break >= 150 %IEC 60811
 >= 195 %
@Temperature 110 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Tear Strength >= 8.00 kN/mBS 6469-99-1
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 90.0 °C
@Time 21600 sec
<50%, Penetration (K=0,7); IEC 60811
Oxygen Index >= 30 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 130 °C
Zone 2 145 °C
Zone 3 160 °C
Zone 4 180 °C
Die Temperature 190 °C
Head Temperature 185 °C
Dry Time 3.00 hour
@Temperature 80.0 °C
 4.00 hour
@Temperature 90.0 °C
 
Descriptive Properties
Corrosivity of gases evolved>4,5 pHIEC 60754-2
Halogen Content< 0,1%IEC 60754-1
Temperature Index Value>300°C21% O2, NES 715
UV ResistanceNo Crack720h, HD 605/A1 2.4.20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS081 / 294165

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.