MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller ElastiSeal® 6098 Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: ElastiSeal® 6098 is a non-flowing sealant designed to waterproof and prevent corrosion in spot weld assem¬blies. This sealant permits welding with conventional spot welders, it prevents moisture and oxygen from en¬tering the joint, and provides corrosion protection to the area that cannot be coated with primer. The sealant dis¬appears from the area of the weld but retains a tight seal around the weld spot, weld strengths are unchanged by the use of ElastiSeal® 6098.

Features:

  • Prevents corrosion in a variety of steel spot welds – Including stainless steel
  • Does not affect weld strength
  • Weldable with conventional spot welders
  • Remains permanently flexible and elastic
  • Will not stain or bleed through most primers and paints
  • Not affected by paint bake temperatures up to 90°C (195°F)
Application: ElastiSeal® 6098 can be applied as a bead or spread as a paste. Welds may be made through the sealer from 10 minutes to 72 hours after application. (“Spitting” may occur if welding is performed before solvent escapes.) This sealer is unaffected by conventional industrial paint bakes. Excess material may be wiped off with mineral spirits; use mineral spirits to clean tools and equipment.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D1475
Solids Content 88 - 92 %ASTM C681
Storage Temperature 4.00 - 32.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time <= 72.0 hourDry Time @ 20°C (68°F) ; 50% RH; ASTM D1640
Shelf Life 24.0 Month
 
Descriptive Properties
ColorAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL129 / 316920

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.