MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic properties. This mix is hot isostatically pressed (HIP'd) into fully dense blocks for further processing into finished blanks and subsequent machining into components.

These materials are used in electronic packaging heat sinks for MCM-L, SEM-E, BGA's, and RF/Microwave applications. The CTE can be controlled by varying the BeO content to match with die materials like GaAs or silicon in RF/microwave applications or match AuSn or AuGe over brazing/soldering temperatures, Kovar, Alloy 46 or 48, and other packaging materials.

Can be machined by conventional processes. Corrosion resistance similar to aluminum. For protection in severe environments such as salt fog, the composite may be coated in a number of ways such as electroless or electrolytic nickel plating, chrome plating, and gold or silver plating for brazing or soldering operations.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 2.05 g/cc
 2.06 g/ccAverage
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity >= 301 GPa
 303 GPaTypical
Fracture Toughness 13.7 MPa-m½Average KIC.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 - 11.0 µm/m-°C
@Temperature 25.0 - 100 °C
 11.5 µm/m-°C
@Temperature 25.0 - 250 °C
average
Specific Heat Capacity 1.584 J/g-°C
Thermal Conductivity >= 200 W/m-K
 210 W/m-KTypical
 
Component Elements PropertiesOriginal ValueComments
BeO 25.8 - 32.25 %
Beryllium, Be 79.37 - 83.5 %As remainder; includes Be from BeO
Oxygen, O 16.5 - 20.63 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
Materion E40 Beryllium/BeO Composite, 40 Volume% BeO
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO
Materion Thermalox® 995 General Purpose 99.5% BeO
Beryllium I-220H Grade 1

NBBC00 / 15310

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.