MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-50278 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-50200 Series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-50278 is a medium hardness, low density, clear grade, available in NAT and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing.

Availability: Asia Pacific

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Processing Stability; Halogen Free; High Clarity; High Purity; Kink Resistant; Low Density; Low Specific Gravity; Medium Hardness; No Animal Derived Components; Radiation (Gamma) Resistant

Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Cast Film

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Oxygen Permeability 1100 cm3 mil/(100 in2 day atm)
@Thickness 1.02 mm
90% RH; ASTM D3985
 1200 cm3 mil/(100 in2 day atm)
@Thickness 1.02 mm
35% RH; ASTM D3985
Density 0.890 g/ccASTM D792
Water Vapor Transmission 2.50 g/100 in²/day
@Thickness 2.54 mm,
Temperature 37.8 °C
100 RH; ASTM F1249
Oxygen Transmission 27.4 cc-mil/100 in²-24hr-atm
@Thickness 1.02 mm
90% RH, Wet; ASTM F1927
 29.5 cc-mil/100 in²-24hr-atm
@Thickness 1.02 mm
35% RH, Wet; ASTM F1927
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
@Time 5.00 sec
ASTM D2240
 81
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 2170 psiASTM D412
Tensile Stress at Strain 645 psi
@Strain 50 %
ASTM D412
 695 psi
@Strain 100 %
ASTM D412
 980 psi
@Strain 300 %
ASTM D412
Elongation at Break 620 %ASTM D412
Tear Strength 367 pliASTM D624
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 83 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 440 °FMelt, Injection
Rear Barrel Temperature 300 - 340 °FInjection
Middle Barrel Temperature 340 - 380 °FInjection
Front Barrel Temperature 380 - 440 °FInjection
Nozzle Temperature 380 - 440 °FInjection
Zone 1 320 - 370 °FExtrusion
Zone 2 360 - 385 °FExtrusion
Zone 3 360 - 400 °FExtrusion
Zone 5 360 - 400 °FExtrusion
Die Temperature 350 - 420 °FExtrusion
Mold Temperature 70.0 - 125 °FInjection
Back Pressure 50.0 - 150 psiInjection
Cushion 0.140 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0738 / 237229

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.