MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extruded and injection-moulded. PEARLTHANE® 11T92EM can be extruded into profiles, belts, tubes and film. In the case of injection moulding, this grade is only recommended for certain specific applications, e.g. when large, hard-to-fill mould cavities are used.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91ASTM D2240
Tensile Strength, Yield 5076 psiASTM D412
Elongation at Break 630 %ASTM D412
100% Modulus 1.16 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.74 ksi
@Strain 300 %
ASTM D412
Tear Strength 570 pliASTM D624 (Die C)
Abrasion 25loss (mm³); DIN 53.516
Compression Set 25 %
@Temperature 22.8 °C,
Time 252000 sec
ASTM D395
 45 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 355 - 375 °FMQSA 111
Glass Transition Temp, Tg -36.0 °FDSC, 10ºC/min; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Feed Temperature 385 °F
Nozzle Temperature 410 °F
Zone 1 390 °FCompression Zone
Zone 2 410 °FMetering Zone
Mold Temperature 95.0 °F
Moisture Content <= 0.10 %MQSA 44
Injection Pressure 1250 psi
Hold Pressure 720 psi
@Time 15.0 sec
Cycle Time - Injection 3.0 sec
Cycle Time - Cooling 30 sec
Screw Speed 180 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer

PMES43 / 88420

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.