MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® (PA66) FR50 BK153J PA66-GF25FR(17)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 25% Glass Reinforced, Flame Retardant, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccDAM; ISO 1183
Water Absorption 0.60 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion; DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 150 cm³/gDS, Sulfuric acid 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaDAM; ISO 527-1/-2
Elongation at Break 2.6 %DAM; ISO 527-1/-2
Tensile Modulus 10400 MPaDAM; ISO 527-1/-2
Flexural Strength 240 MPaDAM; ISO 178
Flexural Modulus 9160 MPaDAM; ISO 178
Poissons Ratio 0.34DAM
Izod Impact, Notched (ISO) 10.7 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact, Notched 9.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 275 VDAM; IEC 60112
Hot Wire Ignition, HWI 300 sec
@Thickness 0.750 mm
DAM; UL 746A
 300 sec
@Thickness 1.50 mm
DAM; UL 746A
 300 sec
@Thickness 3.00 mm
DAM; UL 746A
High Amp Arc Ignition, HAI 166 arcs
@Thickness 0.750 mm
DAM; UL 746A
 171 arcs
@Thickness 1.50 mm
DAM; UL 746A
 187 arcs
@Thickness 3.00 mm
DAM; UL 746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min; 1st heating; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 241 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 80.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 0.350 mm
DAM; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 5VA
@Thickness 1.50 mm
DAM; IEC 60695-11-20
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesFlame retardant
Drying RecommendedyesInjection
FMVSS ClassSE/BISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,GF25 FR(17),M1CF1GR,S14-100
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-GF25FR(17)<ISO 11469
PolymerPA66-GF25 FR(17)
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
Resin IdentificationPA66-GF25FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5416m / 254531

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.