MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Fold™ HP Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Fold M module is designed for high-temperature furnace linings that require corrosion barriers, vapor barriers or just a pre-laid stud pattern. Pyro-Fold M modules are manufactured in three grades of ceramic fiber blanket: HP (Cerablanket), ZR (Cerachem), and CR (Cerachrome). The available combinations of blanket grades, densities, and sizes allow Pyro-Fold M modules to be used in many different types of industrial furnaces. The modules are held to the steel casing by stainless steel studs that are pre-welded to the furnace shell. The PyroFold M module uses a 316 stainless steel nternal support system that was specially designed to allow for quick and reliable installation over coated shells, backup linings and vapor barriers. Pyro-Fold M modules come pre-compressed with restraint banding and an internal support system. Studs, nuts, and installation tools must be orderedseparately. Pyro-Fold Y modules are manufactured from a high-purity blend of raw materials which are used to produce either the HP grade (alumina-silica) or ZR grade (aluminazirconia-silica) ceramic fibers. The Pyro-Fold Y Module utilizes a specially designed 316 SS internal support system and the industry standard Pyro-Bloc stud system. The Pyro-Fold Y Module uses the proven centerfire, one-step weld system which eliminates the need for pre-laid stud patterns. This allows for the fastest installation of any module system now available in the marketplace. The Pyro-Fold Y Module comes complete with internal support system and stud already in place.

Applications:

  • Annealing furnaces
  • Heat treating furnaces
  • Steam flood generators
  • Preheating furnaces
  • Process heaters
  • Ethylene furnaces
  • Reformers
  • Forge furnaces
  • Crude oil heaters
  • Steam flood units
  • Ammonia reformers
  • Tunnel kilns
  • Homogenizing furnaces
  • Heat treating furnaces
  • Shuttle kilns
  • Periodic kilns
  • Homogenizing furnaces
  • Fume incinerators
  • Gas turbin exhaust duct work
  • Pyrolysis heaters

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.128 g/cc
 0.149 g/cc
 0.171 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 260 °C
at 149kg/m3; ASTM C-201
 0.140 W/m-K
@Temperature 538 °C
at 149kg/m3; ASTM C-201
 0.240 W/m-K
@Temperature 816 °C
at 149kg/m3; ASTM C-201
 0.350 W/m-K
@Temperature 1093 °C
at 149kg/m3; ASTM C-201
Melting Point 1760 °C
Maximum Service Temperature, Air <= 1204 °CContinuous
 <= 1316 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 46 %
SiO2 54 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed bar
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
Morgan Advanced Ceramics Cerafelt Refractory Fiber Felt
Morgan Advanced Ceramics Cerachrome™ Blanket Thermal Ceramic

CMORF6461 / 203245

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.