MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Dry Blend E1501 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83ASTM D2240
Tensile Strength, Yield 41.6 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2950 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 79.3 MPaASTM D790
Flexural Modulus 2900 MPaASTM D790
Izod Impact, Notched 85.0 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Compression Molded; ASTM D256A
 520 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded; ASTM D256A
Dart Drop Total Energy 84.5 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 178 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
@Thickness 3.18 mm
Compression Molded, annealed at 50 deg.C; ASTM D648
Flammability, UL94 V-0UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 193 - 204 °C
 
Descriptive Properties
Agency RatingsNSF 51The E1501 white 1564 color is the only NSF 51 listed color in this product.
FeaturesGood Thermal Stability
 Impact Modified
FormsPowder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16354ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesSiding Substrate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL0888 / 145457

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.