MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom PLASTAMID® 6 HI PA6 with improved impact strength  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: PA 6 for injection molding, impacted, modified with thermoplastic elastomer, determined for high impacted moldings also at low temperature. Delivered in natural mode and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccSTN EN ISO 1183-1
Linear Mold Shrinkage 0.0256 cm/cmSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0253 cm/cmSTN EN ISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPaSTN EN ISO 527-2
Elongation at Break 4.0 %STN EN ISO 527-2
Tensile Modulus 1000 MPaSTN EN ISO 527-2
Flexural Strength 40.0 MPaSTN EN ISO 178
Flexural Modulus 1000 MPaSTN EN ISO 178
Charpy Impact, Notched 70.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 70.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °CSTN EN ISO 75-2 (A)
Vicat Softening Point 100 °CSTN EN ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 850 °C
@Thickness 3.00 mm
STN EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
@Time 14400 sec
Moisture Content 0.15 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolene® FPW 10 PPC - 10% Wollastonite Reinforced Polypropylene Copolymer, High Impact Strength
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer
PlastiComp Complet® LGF30 - ETPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced
Gharda Chemicals GAFONE™-P 4300 PPSU, High Impact Strength, High Hydrolysis Resistance
Elix Polymers ELIX ABS P2M-AT Acrylonitrile Butadiene Styrene (ABS), High Impact Strength

PPLACO651 / 140922

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.