Polycarbonate, Flame Retardant, Low Flow Features: • High Impact Resistance • High Viscosity • Self Extinguishing Process: Injection Molding Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |