MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-CH-61 Anti Yellowing
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-CH-61 can be applied for all kinds of resin and polymer that can prevent the aging and thermochromic in the processing. In addition, GY-CH-61 can decrease the yellowing that would be the best solution to the discoloration problems.

Features:

  • Improves the discoloration of polymer while processing in the high temperature.
  • Stabilizes the resin and polymer
  • Prevents the thermal-oxidative degrade of resin and plastic in the process of aging
  • Highly effective and low additive value.
  • Low volatility, won’t migration
  • Well function of hydrolysis
  • Prevents the discoloration of resin due to the heating
  • Improves the decreasing physical properties of resin while in the process of aging
Applications:
  • PU synthetic leather, resin, PU foam, TPU injection, extrusion, hot melting and blow mold
  • The properties of PU(RIM) , PU super fiber, anti-fouling, plastic sealing
  • HDPE, PP, LLDPE, PES, Hydrocarbon accumulation product
  • Polyoxymethylene(POM) , Polyamide?polyester, industrial plastic
  • PVC?ABS?varieties kind of use in plastic industry

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.530 - 0.630 g/cc
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Descriptive Properties
AppearancePowder
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN506 / 266814

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.