MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kazanorgsintez Carbanox SKD-10 Polyethyleneglycol Mixture
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Production Method: Obtained by interaction of oleic acid and ethylene oxide.

Application: Intended for use from 3% to 5% water emulsions as antistatic, lubricating and finishing agent for chemical fibers, natural and mixed fibers, as well as softener in the production of flax-fibers as a dispersing agent or emulsification agent for different dispersing media and as a degreaser in detergents.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0mg of KOH/g, Grades A and B
 
Component Elements PropertiesOriginal ValueComments
Free Water <= 1.5 %Grade A
 <= 10 %Grade B
 
Descriptive Properties
AppearanceViscous oily brown liquid
Saponification Number, mg of KOH65-85Grades A and B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type H12 Hot Work Tool Steel
AISI Type A2 Tool Steel
Lanxess Aflux® 42 M pellets Processing Aid
Lanxess Aflux® 42 M Processing Aid
Lanxess Aflux® 42 Processing Aid

PKAZAN125 / 127444

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.