MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Chirulen® 1050 MediTECH Compression Molded UHMWPE Form  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: MediTECH Compression Molded UHMWPE Form, produced from Celanese GUR 1050 resin. ISO Cell Designation: Thermoplastic ISO 11542-PE-UHMW QD, 2-2-2, ASTM Cell Designation: S-UHMW-PE0111A111 Material evaluated based on ISO 5834-1 Type 1, ISO 5834-2 Type 1, and ASTM F648 Type 1.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.931 g/ccASTM D792
Water Absorption <= 0.050 %ASTM D570
Oxidative Induction Time (OIT) 10 min
@Temperature 200 °C
ASTM D3895
Crystallinity 55 %1st heat, 20°C - 160°C; ASTM F2625
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66
@Time 15.0 sec
ASTM D2240
Tensile Strength, Ultimate 54.6 MPaASTM F648 /ASTM D638
Tensile Strength, Yield 21.1 MPaASTM F648 /ASTM D638
Elongation at Break 417 %ASTM F648 /ASTM D638
Charpy Impact Unnotched 101 kJ/m²ISO 11542-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM D696
Thermal Conductivity 0.400 W/m-KDIN 52612
Melting Point 137 °C10°C / min; ASTM DF2625
Crystallization Temperature 126 - 144 °CASTM F2625
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CASTM D648
Vicat Softening Point 135 °C
@Load 1.02 kg
50 °C/Hr.; ASTM D1525 B
 
Descriptive Properties
Oxidation Resistance<0.1ASTM F2102, Surface Oxidation Index
 <0.1ASTM F2102, Bulk Oxidation Index

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM932 / 291089

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.