MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Eastman CM01 PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.

Applications/Uses

  • Carbonated soft drink containers
  • Food Packaging
  • Bottles
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Bulk Density 0.858 g/ccPoured; ASTM D1895
     0.931 g/ccVibrated; ASTM D1895
    Density 1.40 g/ccCrystalline Density; ASTM D1505
    Melt Density 1.20 g/cc
    @Temperature 285 °C
    ASTM D1238
    Viscosity Measurement 0.79 - 0.83Intrinsic; EMN-A-AC-G-V-1
     
    Thermal PropertiesOriginal ValueComments
    Heat of Fusion 57.0 J/gASTM E793
    Specific Heat Capacity 1.10 J/g-°CASTM E1269
     1.30 J/g-°C
    @Temperature 80.0 °C
    ASTM E1269
     1.50 J/g-°C
    @Temperature 100 °C
    ASTM E1269
     1.80 J/g-°C
    @Temperature 200 °C
    ASTM E1269
     2.00 J/g-°C
    @Temperature 280 °C
    ASTM E1269
    Melting Point 241 °CCrystalline Peak; ASTM D3418
     
    Descriptive Properties
    Acetaldehyde<1ppmTEPO-A-AN-G-GC-67
    Color, CIE a*-2.5 to 0.5VGAS-A-AN-G-RS-001
    Color, CIE b*-2.6 to -0.2VGAS-A-AN-G-RS-001
    Color, CIE L*81 minVGAS-A-AN-G-RS-001
    Fines, wt%, max0.1VGAS-A-AN-G-GA-1
    Pellet ShapeCylindrical, 2x2x3 mm

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Invista 2201 PET Copolymer Packaging Resin
    Invista 1101 PET Copolymer Packaging Resin
    Eastman Aqua 18696 PET
    Eastman 9921 PET Injection Molded
    Dow LIGHTER™ C88 Polyethylene Terephthalate (PET) Resin

    PE9145 / 35202

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.