Vacuum formed products are rigid, self-supporting fiber insulation manufactured from a slurry of ceramic fibers, binders and other proprietary ingredients. Customers are provided with optimized, engineered solutions from our wide range of formulations. Kaowool 2600 uses high temperature alumina fibers in the manufacturing process. It is an excellent dimensionally stable product and has minimal shrinkage at its use limit of 2700°F (1510°C).Information provided by Morgan Advanced Materials |