MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton MRS 5 Metal Rebuilding System
Categories: Ceramic

Material Notes: MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as well as rebuild worn surfaces quickly, returning the damaged component back to service faster than conventional welding. MRS 5 is designed to cure underwater. It is normally applied at a thickness of 3 mm (1/8”) or more. MRS 5 is 100% solids, non-shrinking.

Benefits:

  • Exceptional resistance to permeation in water immersion
  • Excellent leak repair compound due to high build characteristics in single coat application with rapid cure
  • Cures underwater
  • Tough resin structure resist thermal-mechanical shock
  • Outstanding adhesion insures reliable performance
  • Labor and downtime are reduced due to ease of application and rapid curing
  • Convenient 4 -1 mix ratio and verification of mix by color change
  • Cures at temperatures as low as 4°C (40°F)

Suggested Uses:

  • Condensers
  • Cooling Water Pumps
  • Flange Faces
  • Pump Volutes
  • Valve Bodies
  • Pneumatic Transport Lines
  • Pipe Elbows
  • Pitted Pipes
  • Heat Exchangers
  • Pitted Tanks and Vessels

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ASTM D2240
Tensile Strength at Break 2580 psiASTM D638
Flexural Strength 3900 psiASTM D790
Flexural Modulus 420000 psiASTM D790
Compressive Strength 9000 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 66.0 °CWet
 93.0 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 hour
@Temperature 32.0 °C
Light Load
 0.330 hour
@Temperature 25.0 °C
Light Load
 0.4167 hour
@Temperature 32.0 °C
Full Load
 0.583 hour
@Temperature 16.0 °C
Light Load
 0.750 hour
@Temperature 25.0 °C
Full Load
 0.830 hour
@Temperature 4.00 °C
Light Load
 1.00 hour
@Temperature 32.0 °C
Full Chemical
 1.00 hour
@Temperature 16.0 °C
Full Load
 1.25 hour
@Temperature 4.00 °C
Full Load
 2.00 hour
@Temperature 25.0 °C
Full Chemical
 3.00 hour
@Temperature 16.0 °C
Full Chemical
 8.00 hour
@Temperature 4.00 °C
Full Chemical
Tack-Free Time 0.1167 hour
@Temperature 32.0 °C
 0.167 hour
@Temperature 25.0 °C
 0.330 hour
@Temperature 16.0 °C
 0.500 hour
@Temperature 4.00 °C
 
Descriptive Properties
ColorMedium-Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay
Aluminum Ammonium Sulfate Dodecahydrate, AlNH4(SO4)2-12H2O

PPTCHS127 / 138239

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.