MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Bayhydur® XP 2700 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Hydrophilic aliphatic polyisocyanate based on hexamethylene diisocyanate (HDI). As a hardener for aqueous two component polyurethane systems.

Properties / Applications: Bayhydur® XP 2700 is a crosslinker for aqueous coatings. It was developed specially for trade applications where the ease of mixing the hardener by manual stirring is a key requirement.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccDIN 51 757
Volatiles 33 - 37 %2.2 g / 120 min / 100°C; DIN EN ISO 3251
Viscosity 62 - 92 cPD = 200 s-1; DIN EN ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point 61.0 °CDIN EN ISO 2719
 
Descriptive Properties
Color<150Hazen, DIN EN 1557
Content<0.1%Monomeric HDI, DIN EN ISO 10283
 10.3-10.9%NCO, DIN EN ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0203 / 201986

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.