Sandvik Ti Grade 9 (Sandvik Ti 3Al2.5V) is a titanium grade characterized by excellent corrosion resistance to seawater and higher mechanical properties than stainless steels. The Ti32.5 alloy is characterized by:- Excellent resistance to general corrosion in seawater applications
- High mechanical strength, superior strength to weight ratio
- Resistant to stress corrosion cracking in chloride and sour gas environments
- Excellent resistance to pitting, crevice and erosion corrosion
- Good formability and weldability
- Very low thermal expansion
- Excellent fatigue properties from Sandvik's proprietary processing that controls crystal texture
Information provided by Sandvik |