MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil DDU-4330 Unrestricted Drug Delivery Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Comments: Low Consistency Elastomer

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Viscosity 115000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25
Tensile Strength at Break 4.83 MPa
Elongation at Break 525 %
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 150 °C
Post, Stabilized for >3 hrs
 3.00 min
@Temperature 150 °C
 
Descriptive Properties
ColorTranslucent Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
AISI E4340 Steel, annealed 810°C (1490°F)
AISI E4340 H Steel, oil quenched 845°C, 425°C (800°F) temper
AISI E4340 H Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round

PNUSIL470 / 142194

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.