MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • Strong flexible bonds
  • High viscosity grade adhesive for many brush or spray applications.
  • Quick drying
  • Excellent resistance to many fuels and oils
  • Bond leather, nitrile rubber, most plastics, gasketing materials to a variety of substrates
  • May be heat cured to obtain improved physical properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 46 - 55 %
Brookfield Viscosity 35000 - 90000 cPRVF #6 sp @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 9.00 psi
@Temperature 82.0 °C
Overlap, 1/8" Birch/Birch
 20.0 psi
@Temperature 66.0 °C
Overlap, 1/8" Birch/Birch
 152 psi
@Temperature 1.00 °C
Overlap, 1/8" Birch/Birch
 200 psi
@Temperature 14.0 °C
Overlap, 1/8" Birch/Birch
Peel Strength 4.00 pli
@Temperature 14.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 9.00 pli
@Temperature 82.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 13.0 pli
@Temperature 14.0 °C,
Time 86400 sec
180°, Canvas/Steel
 16.0 pli
@Temperature 66.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 20.0 pli
@Temperature 1.00 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 23.5 pli
@Temperature 14.0 °C,
Time 259000 sec
180°, Canvas/Steel
 27.5 pli
@Temperature 14.0 °C,
Time 432000 sec
180°, Canvas/Steel
 31.0 pli
@Temperature 14.0 °C,
Time 605000 sec
180°, Canvas/Steel
 35.0 pli
@Temperature 14.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
 
Thermal PropertiesOriginal ValueComments
Flash Point -18.0 °CCC
 
Descriptive Properties
AppearanceDark Brown
BaseNitrile Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive
3M Scotch-Grip™ 847 Rubber and Gasket Adhesive 847

PMM34121 / 168868

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.