MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Almag® Oil
Categories: Fluid; Lubricant

Material Notes: Texaco Almag oil delivers value through:
  • Low viscosity that provides faster wetting of metal surfaces and penetration to the cutting zone.
  • Excellent cooling properties, carrying heat away from the cutting zone.
  • Excellent lubricity at the chip-tool interface, reducing frictional heat, improving tool life and surface finish.

Texaco Almag oil is a low viscosity, nonactive cutting oil for use in light duty machining and grinding operations on ferrous and nonferrous metals. It is particularly useful on aluminum, magnesium and their alloys.

Texaco Almag Oil is a straight mineral oil. It is a light-colored oil that possesses excellent cooling properties and high dielectric strength. Because of its composition, it is nonstaining for ferrous and nonferrous surfaces. It gives good wetting and penetration of cutting surfaces.

Texaco Almag oil is recommended for light duty machining and grinding operations on ferrous and nonferrous metals. It is excellent for aluminum, magnesium and their alloys. It is particularly suited for the machining of magnesium where the use of a water-based fluid could create a fire hazard.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221564; MSDS Number: 10275

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 28 °
Viscosity Measurement 33Viscosity Index
Saybolt Viscosity at 100°F 60 SUS
Saybolt Viscosity at 210°F 34 SUS
Kinematic Viscosity at 40°C (104°F) 9.5 cSt
Kinematic Viscosity at 100°C (212°F) 2.33 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -56.0 °C
Flash Point 146 °C
 
Descriptive Properties
Fatty OilNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® SDS Surfactant
ChevronTexaco Almag® Special

WTEXA280 / 77159

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.