MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate flexibility and faster cycles. Excellent thermal and chemical resistance properties provided by the polyamide backbone. It demonstrates the highest impact performance within the Capron copolymer product line while maintaining an excellent balance of strength and stiffness. Excellent chemical resistance to greases, oils and hydrocarbons.

Capron 8351 HS Bk-102 is generally recommended for applications such as spray gun and power tool handles, trim clips and fasteners, wall anchors and automotive roof clips rack components. ASTM Callout PA263 + PA0220 B32310.

Data provided by Allied Signal.

Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of 10-95 degC (50-203 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO data
Water Absorption 1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.9 %50% RH; 23°C; ISO data
Water Absorption at Saturation 6.7 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.0050 cm/cmISO data
 0.014 cm/cmASTM data MD
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 53.0 MPaISO value at 50 mm/min.
 55.0 MPaASTM value at 50 mm/min.
Elongation at Break >= 50 %Nominal
 >= 100 %Nominal
Flexural Modulus 1.40 GPaISO Value
 1.69 GPaASTM Value
Poissons Ratio 0.35ISO data
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cmISO data
 
Thermal PropertiesOriginal ValueComments
CTE, linear 106 µm/m-°C
@Temperature 20.0 °C
ASTM data
Melting Point 220 °CASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CASTM Data
Flammability, UL94 HB
@Thickness 0.810 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 275 °CSee Materials Notes
Mold Temperature 95.0 °CSee Materials Notes
Drying Temperature 85.0 °CSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALD15 / 23909

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.