MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SCIGRIP SG5000-06 A Methacrylate Adhesive + SG5000-06 B Activator
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: SCIGRIP® SG5000 Series Methacrylate Adhesives are high strength two-component products for bonding metals, plastics and composites. They offer a unique combination of convenient 1:1 non-critical mix ratio and ability to adhere to a wide variety of materials. Most metals, including steel and aluminum, can be bonded without surface pretreatment. A choice of 3, 6 and 15 minute working times, fast cure and rapid strength build make this series of adhesives an ideal first choice for diverse bonding applications.

Features: Primerless metal bonding for most metals; Minimal surface preparation; Excellent environmental & chemical resistance

Information provided by SCIGRIP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccAdhesive
 0.970 g/ccActivator
 0.970 g/ccMix
Viscosity 90000 - 150000 cPAdhesive
 150000 - 250000 cPActivator
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 5.10 - 5.80 ksi
Elongation at Break 5.0 - 10 %
Tensile Modulus 160 - 180 ksi
Adhesive Bond Strength 2610 - 3630 psiLap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 212 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 12.0 min
@Temperature 23.9 °C
Fixture Time
Working Life 5.00 - 8.00 min
@Temperature 23.9 °C
 
Descriptive Properties
ColorAmberAdhesive
 Amber or BlackActivator
 Amber or BlackMix
Mix Ratio1:1 A:BNon critical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIGR968 / 243192

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.