MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon SMCA granules Sodium monochloroacetate
Categories: Other Engineering Material

Material Notes: This monochloroacetic acid solid are supplied as white granules. It is used as an essential raw material for a variety of products, such as carboxymethyl cellulose, adhesives, pharmaceuticals and crop protection chemicals.

CAS number: 3926-62-3

Applications: Main uses include production of: MCA esters, carboxymethyl cellulose, carboxymethyl starch, thioglycolic acid, cyanoacetic acid (incl. esters), barbiturates, malonic acid (incl. esters and derivates), vitamins, sequestering agents (EDTA), glycine, dyes (indigo and derivates), chloroacetylchloride (CAC), surfactants

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.20 %in MCA
 
Descriptive Properties
AppearanceWhite granules
Content= 0.2 %Sodium dichloroacetate
 = 0.2 %Sodium acetate
 = 0.7 %Sodium chloride
 = 10 mg/kgIron
 = 98.0 %Sodium monochloroacetate, incl. MCA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY870 / 286393

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.