MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR C4210HF PC+ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 37 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ISO 2039-2
Ball Indentation Hardness 116 MPaISO 2039-1
Tensile Strength at Break 85.0 MPa5 mm/min; ASTM D638
 90.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 85.0 MPa5 mm/min; ASTM D638
 90.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ASTM D638
 3.2 %5 mm/min; ISO 527
Elongation at Yield 3.0 %5 mm/min; ASTM D638
Tensile Modulus 4700 MPa1mm/min; ISO 527
 4900 MPa5 mm/min; ASTM D638
Flexural Strength 135 MPa2 mm/min; break; ISO 178
 140 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 125 MPa2 mm/min; ISO 178
Flexural Modulus 4250 MPa2 mm/min; ISO 178
 4300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 75.0 J/mASTM D256
 60.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 480 J/mASTM D4812
 480 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 JASTM D3763
 8.00 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 134 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 128 °C
@Thickness 6.40 mm
unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10781 / 244248

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.