Features and Typical Applications Ability to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in harsh environments. Typical applications include sensors, transformers, power supplies, and rectifiers.
Emerson & Cuming W-66/17M-1 Stycast® Two-Component Epoxy High Service Temp Encapsulant Excellent Chemical Resistance. Mix Ratio by Weight = 100:40 Cure Type: Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |