MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ohara Clearceram-Z® Ultra Low Expansion Glass Ceramic
Categories: Ceramic; Machinable Ceramic

Material Notes: Clearceram-Z® shows almost Zero Thermal Expansion over a wide temperature range and offers superior thermal shock resistance. CCZ Regular offers lower thermal expansion across a wide temperature range, while the CCZ HS offers lower thermal expansion near room temperature. It is comprised of approximately 70% ceramic, which makes the mechanical characteristics superior to regular amorphous glass when comparing properties such as Young´s Modulus, Rigidity, Bending Strength, and Hardness. It has superior machinability and chemical properties.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.55 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 600
Hardness, Vickers 680
Modulus of Elasticity 90.0 GPa
@Temperature -50.0 - 300 °C
Modulus of Rigidity 36.0 GPa
@Temperature -50.0 - 300 °C
Flexural Strength 116 MPa4-point bending strength; JIS R1601
Poissons Ratio 0.25
Abrasion 62Aa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.60e+8 ohm-cm
@Temperature 200 °C
 1.50e+12 ohm-cm
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.100 - 0.100 µm/m-°C
@Temperature 0.000 - 50.0 °C
Guaranteed
 0.0200 µm/m-°C
@Temperature -60.0 - 160 °C
Typical
Specific Heat Capacity 0.777 J/g-°C
Thermal Conductivity 1.51 W/m-K
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5535nF' (Cd F' line)
 1.52441
@Wavelength 1813.07 nm
 1.528
@Wavelength 1550 nm
 1.52819
@Wavelength 1529.58 nm
 1.5334
@Wavelength 1128.64 nm
 1.54357
@Wavelength 643.85 nm
nC' (Cd C' line)
 1.546
@Wavelength 587.56 nm
nd (He D line)
 1.54607
@Wavelength 546.07 nm
ne (Hg e line)
 1.55838
@Wavelength 435.835 nm
ng (Hg g line)
 1.563
@Wavelength 404.656 nm
nh (Hg h line)
Abbe Number 55.5ν d
Transmission, Visible >= 85 %
@Thickness 10.0 mm,
Wavelength 500 nm
Internal Transmission
 95 %
@Thickness 10.0 mm,
Wavelength 600 nm
Internal Transmission
 98 %
@Thickness 10.0 mm,
Wavelength 700 nm
Internal Transmission
IR Transmittance 88 %
@Thickness 10.0 mm,
Wavelength 2500 nm
Optical Transmission
 91 %
@Wavelength 850 - 2100 nm,
Thickness 10.0 mm
Optical Transmission
 >= 98 %
@Thickness 10.0 mm,
Wavelength 980 nm
Internal Transmission
 >= 98 %
@Thickness 10.0 mm,
Wavelength 1550 nm
Internal Transmission
 99 %
@Wavelength 800 - 1600 nm,
Thickness 10.0 mm
Internal Transmission
 
Descriptive Properties
Acid Resistance, Powder Method, RA(P)1
Alkali Resistance (Powder), Ralk (%)0.25
Water Resistance, RW(P)2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CZOHARA786 / 281625

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.