MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Trough Grease Soft
Categories: Fluid; Lubricant; White Mineral Oil (WMO)

Material Notes: Chevron Trough Grease Soft is a soft petrolatum formulation used to grease the sides of troughs in which dough is allowed to rise, which prevents the dough from adhering to the sides.

Applications

Chevron Trough Grease Soft may be used for food applications where the U.S. Food and Drug Administration (FDA) has approved this type of product. These applications include use as a:

  • release and sealing agent for confectioneries
  • protective coating on raw fruits and vegetables
  • defoaming agent for beet sugar production, 21 CFR 172.880(c).
Non food applications include for example, use as a nonstaining concrete from lubricant.

Key Words: CPS Number: 231031; MSDS Number: 7196
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 210°F 42 SUS
Kinematic Viscosity at 100°C (212°F) 5.7 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Flash Point 177 °CASTM D92
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Color1Y, Lovibond 2" cell, IP 17
Congealing Point °C38
Consistency 25°C290

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV131 / 74746

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.