16017b3906a94e2c9fd52bb7a0833749Easily cold formed by heading, extruding, upsetting, bending, and other deforming processes. Uses for wires include electroplated products, such as racks, storage bins, shopping carts, fan guards, and jewelry, and unplated such as wires, staples, hardware, and barbed wire. |
UNS G10120, AISI1012, ASTM A29, ASTM A510, ASTM A519, ASTM A545, ASTM A549, ASTM A575, ASTM A576, MIL SPEC MIL-S-11310 (CS1012), SAE J403, SAE J412, SAE J414 |