MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Maxxam® FR PP FR 8-6a Polypropylene (PP), Talc Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Description/Features:

  • Flame Retardant
  • Talc Filled
  • Low Flow
  • Impact Modified
  • Medium Impact
  • UL 94 V0
  • UL 94 5VA
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Melt Flow 7.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A - Manual Operation; ASTM D1238
 7.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Procedure A - Manual Operation; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2600 psiType 1 - Rigids; 2 in/min; ASTM D638
 3800 psiType 1 - Rigids; 2 in/min; ASTM D638
Elongation at Break 25 %Type 1 - Rigids, 2 in/min; ASTM D638
 36 %Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Strength 3600 psiASTM D790
Flexural Modulus 250000 psiASTM D790
 400000 psiASTM D790
Izod Impact, Notched 0.600 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
 2.20 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
Gardner Impact 1.667 ft-lb0.125 in.; ASTM D3029
 12.5 ft-lb0.125 in.; ASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 194 °FUnannealed; ASTM D648
 248 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.787 mm
All Colors; UL 94
 V-0
@Thickness 0.787 mm
All Colors; UL 94
 5VA
@Thickness 2.39 mm
All Colors; UL 94
 5VA
@Thickness 3.17 mm
All Colors; UL 94
Oxygen Index 27 %0.125 in. bars; ASTM D2863
 27 %0.125 in. bars; ASTM D2863
 
Descriptive Properties
Product FormPellets
 Pellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled
Washington Penn Homopolymer Polypropylene 10% Talc Filled
Mytex Polymers AS23KW-01 Polypropylene, Talc filled, Compounded
Avient Maxxam® BD-418.G001 Polypropylene (PP), Talc Filled
A. Schulman LPP40YR04BK 40% Calcium Carbonate Filled, Copolymer Polypropylene

PH1PO2634 / 44651

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.