MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Krytox™ EG 3000 PFPE Electronic Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Krytox™ EG 3000 grease is formulated specifically for electrical applications. While this grade offers different viscosities to match the application in which it is being used, it is: Clear, colorless, fluorinated synthetic greases, Nonreactive and nonflammable, Safe in environments with chemical and oxygen service, Long lasting.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.93 g/cc
@Temperature 25.0 °C
Volatiles 3.0 %
@Treatment Temp. 260 °C,
Time 79200 sec
D972
Viscosity Measure 6.0 cSt
@Temperature 204 °C
base oil; D445
 43 cSt
@Temperature 99.0 °C
base oil; D445
 500 cSt
@Temperature 38.0 °C
base oil; D445
 1600 cSt
@Temperature 20.0 °C
base oil; D445
Vapor Pressure 6.00e-9 torr
@Temperature 38.0 °C
Knudsen
 0.000300 torr
@Temperature 260 °C
Knudsen
Evaporation Loss 1.0 %
@Temperature 204 °C,
Time 79200 sec
FTMS 791B 350.1
 6.0 %
@Temperature 260 °C,
Time 79200 sec
FTMS 791B 350.1
 
Mechanical PropertiesOriginal ValueComments
Penetration 265 - 29560 strokes; ASTM D217
Oil Separation 3.0 %
@Treatment Temp. 99.0 °C,
Time 108000 sec
% wt; FTMS 791B 321.1
 10 %
@Treatment Temp. 204 °C,
Time 108000 sec
% wt; FTMS 791B 321.1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 316 °C
Minimum Service Temperature, Air -29.0 °C
Pour Point -30.0 °Cbase oil; D97
 
Descriptive Properties
Appearancebuttery
Liquid Oxygen ImpactPassASTM D2512, NASA MSFC 106B
Mechanical StabilityNo change from original gradeASTM D217, 10,000 St, 100,000 Strokes
Oxidation Stability0 psig O2 pressure dropAfter 600 hr. 99°C. ASTM D942

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ864 / 254053

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.