MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ COLORCOMP™ Compound A1000FXB Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP COLORCOMP A1000FXB compound is based on unfilled Acrylonitrile Butadiene Styrene (ABS) resin. Added features of this grade include: Healthcare, Biocompatible (ISO10993), Low Extractables, Gamma & EtO Sterilizable, Superior Molding.

Features: Low Extractable,Aesthetics and Appearance,Healthcare,Steam, Gamma, EtO and E-beam sterilizable,Superior Molding,Custom Color,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Density 1.05 g/ccISO 1183
Moisture Absorption 0.100 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 5.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 19 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 33.0 MPa5 mm/min; ASTM D638
 35.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 44.0 MPa5 mm/min; ASTM D638
 50.0 MPa5 mm/min; ISO 527
Elongation at Break 24 %5 mm/min; ASTM D638
 24.8 %5 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ASTM D638
 2.6 %5 mm/min; ISO 527
Tensile Modulus 2270 MPa5 mm/min; ASTM D638
 2530 MPa1 mm/min; ISO 527
Flexural Strength 72.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 76.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
 2410 MPa2 mm/min; ISO 178
Izod Impact Notched 320 JASTM D256
 133 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 23.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Dart Drop, Total Energy 30.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
UL 746A
 15 - 30 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 98.0 °CRate B/50; ASTM D1525
 100 °CRate B/50; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 260 °C
Zone 2 205 - 225 °C
Zone 3 215 - 240 °C
Melt Temperature 220 - 260 °CInjection Molding
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80517 / 288464

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.