- Specially formulated high temperature brazing flux.
- For use on ferrous alloys, stainless steels, carbides, and other specialty alloys.
- Residues are water-soluble.
- Fluoride-free formulation
Description: Superior No. 615 is a high temperature brazing paste flux that is active and protective to 1,205ºC/2,200ºF. It is specially formulated to meet the process requirements of high-temperature filler alloys, such as manganese-containing alloys, low-fuming bronze (CDA 681) and nickel-silver (CDA 773). It is recommended for joining carbide to stainless steel, ferrous alloys, and other alloys requiring high temperature brazing.Applications: Superior No. 615 is a boron-modified brazing flux used with high-temperature alloys for manufacturing a wide variety of products including; carbide mining tools, snowplow blades, stainless steel, large steel parts, or processes requiring a long heating cycle. Information provided by Superior Flux |