MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Borealis Queo™ 0219 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Queo 0219 is an ethylene based octene-1 plastomer, produced in a solution polymerization process using a metallocene catalyst. CAS-No. 26221-73-8

Special Features:

  • Versatile blending with other polyolefins in film, extrusion and molding applications
  • Outstanding toughness
  • Outstanding puncture resistance
  • Low temperature impact strength
  • High flexibility and surface softness
  • High clarity
Applications:
  • High clarity PP molded goods
  • Masterbatches and compounds
  • Extrusion coating
Additives: Queo 0219 contains processing stabilizers

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccISO 1183
Viscosity 30.0 cP
@Shear Rate 10000 1/s,
Temperature 230 °C
DIN 54811
 40.0 cP
@Shear Rate 10000 1/s,
Temperature 190 °C
DIN 54811
 140 cP
@Shear Rate 100 1/s,
Temperature 230 °C
DIN 54811
 400 cP
@Shear Rate 100 1/s,
Temperature 190 °C
DIN 54811
Environmental Stress Crack Resistance >= 1000 hourASTM D 1693-B
Melt Flow 19.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38.0ISO 868
Tensile Strength 13.0 MPaISO 527-2
Elongation at Break 930 %ISO 527-2
Flexural Modulus 63.0 MPaISO 178
Izod Impact, Notched (ISO) NBISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 97.0 °CISO 11357-3
Vicat Softening Point 71.0 °C
@Load 1.02 kg
ISO 306
Brittleness Temperature <= -90.0 °CASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9890 / 323247

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.