MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Meets ISO 10993 and/or USP Class VI biocompatibility requirement. Ecdel™ elastomers are plasticizer free copolyester elastomers (COPE ) that offer clarity, toughness, flexibility, and chemical resistance for flexible packaging including medical and pharmaceutical applications. Ecdel™ elastomer 9967 may be processed on standard injection molding, extrusion blow molding, profile extrusion, extrusion coating, or film extrusion equipment. Ecdel™ elastomers may be extrusion blow molded directly into bags or extruded into blown or cast film for later fabrication into bags. Ecdel™ elastomers are radiation, electron beam, ethylene oxide, and autoclave sterilization stable. 9967's high inherent viscosity may be helpful where good melt strength is required (blown film or profile extrusion).This product has been CRADLE TO CRADLE CERTIFIED cm Silver.

Applications/Uses:

  • Bags
  • Flexible medical
  • Flexible packaging
  • IV Containers
  • Pharmaceutical packaging
  • Tubing
Key Attributes:
  • Chemical resistant with low extractables
  • Excellent clarity
  • Excellent toughness & flexibility without plasticizers
  • Heat & sterilization stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
Water Absorption 0.40 %
@Time 86400 sec
ASTM D570
Water Vapor Transmission 132 g/m²/day
@Temperature 38.0 °C
Film property at 0.13 mm; ASTM F372
Oxygen Transmission 841 cc-mil/100 in²-24hr-atm
@Temperature 30.0 °C
Film property at 0.13 mm; ASTM D1434
Viscosity 1.23 cPInherent, EMN-A-AC-GV- 1
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Hardness, Shore D 55ASTM D2240
Tensile Strength at Break 23.0 MPaASTM D638
Film Tensile Strength at Yield, MD 11.2 MPaFilm property at 0.13 mm; ASTM D882
Tensile Strength, Yield 13.0 MPa500 mm/min; ASTM D638
Film Elongation at Break, MD 330 %Film property at 0.13 mm; ASTM D882
Film Elongation at Break, TD >= 550 %Film property at 0.13 mm; ASTM D882
Film Elongation at Yield, MD 46 %Film property at 0.13 mm; ASTM D882
Film Elongation at Yield, TD 20 %Film property at 0.13 mm; ASTM D882
Elongation at Break 400 %ASTM D638
Elongation at Yield 38 %ASTM D638
Tensile Modulus 0.170 GPaASTM D638
 0.197 GPaTD, Tangent, Film property at 0.13 mm; ASTM D882
 0.221 GPaMD, Tangent, Film property at 0.13 mm; ASTM D882
Flexural Modulus 0.150 GPaASTM D790
Izod Impact, Notched 40.0 J/m
@Temperature -40.0 °C
ASTM D256
Coefficient of Friction >= 1.0ASTM D1894
Tear Strength, Total 350 NASTM D1004
Film Tensile Strength at Break, MD 41.5 MPaFilm property at 0.13 mm; ASTM D882
Film Tensile Strength at Break, TD 18.1 MPaFilm property at 0.13 mm; ASTM D882
Torsional Stiffness 240 MPa
@Temperature -28.0 °C
Modulus; ASTM D1043
 930 MPa
@Temperature <=-70.0 °C
Modulus; ASTM D1043
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 27.0 J/gASTM E793
CTE, linear 15.0 µm/m-°CASTM D696
Specific Heat Capacity 1.60 J/g-°C
@Temperature 25.0 °C
solid
 1.80 J/g-°C
@Temperature 100 °C
solid
 2.00 J/g-°C
@Temperature 150 °C
solid
 2.30 J/g-°C
@Temperature 175 °C
solid
 2.30 J/g-°C
@Temperature 225 °C
melt
 3.10 J/g-°C
@Temperature 200 °C
transition
Thermal Conductivity 0.190 W/m-KASTM C177
Melting Point 205 °C
Crystallization Temperature 140 °CTemperature on Cooling
Vicat Softening Point 170 °C1 kg load; ASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
Glass Transition Temp, Tg -3.00 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51Film property at 0.13 mm; ASTM D542
Haze 1.0 %
@Thickness 0.130 mm
Film; ASTM D1003
Gloss 73 %45°, Film property at 0.13 mm; ASTM D2457
Transmission, Visible 91 %Regular, Film property at 0.13 mm; ASTM D1003
 94 %Transmittance, Film property at 0.13 mm; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer
Eastman AP007 Copolyester
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer
Eastman Neostar FN006 Elastomer
Eastman Neostar FN005 Elastomer

PEAT6055_B / 217528

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.