MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP5035 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen HP5035 is a polypropylene homopolymer with excellent processability and high mechanical properties, typical customer application is LWRT (low weight reinforced thermoplastic) of automotive parts. Applications: Automotive Parts, Exterior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
Melt Flow 100 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102
Tensile Strength, Yield 33.0 MPa
Elongation at Yield 8.0 %
Flexural Modulus 1400 MPa
Izod Impact, Notched 20.0 J/m
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zoltek™ OX FS 06 X 3 Oxidized PAN Fiber Scrim Fabric
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-T800-5H-280 GSM 5 Harness Carbon Fabric

PEQT9023 / 220654

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.