MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Skybond® 6000 Aromatic Polyimide Resin for RTM Molding
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Produces RTM composites with outstanding thermal resistance.

Information provided by Industrial Summit Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content >= 98 %Resin
Viscosity <= 1000 cP
@Temperature 250 °C
Melt
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 114.3 ksiG30 Fabric Composite; ASTM D3039
Flexural Strength 97.0 ksi
@Temperature 23.0 °C
T650-35 12K HS Fabric / G30 Fabric Composite; ASTM D7264
 126 ksi
@Temperature 204 °C
T650-35 12K HS Fabric / G30 Fabric Composite; ASTM D7264
 146 ksi
@Temperature 176 °C
T650-35 12K HS Fabric / G30 Fabric Composite; ASTM D7264
Flexural Modulus 5650 ksiT650-35 12K HS Fabric / G30 Fabric Composite; ASTM D7264
Compressive Strength 98.3 ksiT650-35 12K HS Fabric Composite; ASTM D3410M
Shear Strength 5.68 ksi
@Temperature 200 °C
Short Beam; T650-35 12K HS Fabric / G30 Fabric Composite; ASTM D2344
 9.24 ksi
@Temperature 23.0 °C
Short Beam; T650-35 12K HS Fabric / G30 Fabric Composite; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 235 °CComposite
 250 - 260 °CResin
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 - 250 °CRTM Molding Injection Temperature
 335 °CRTM Molding; alternate 2-4 hour cure
 350 °CRTM Molding 1-2 hour cure
Injection Pressure 140 - 250 psiRTM Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Oxygen-free electronic Copper, UNS C10100
Copper, Cu; Annealed
Copper, UNS C12000
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H10 Temper flat products

PISTEC970 / 183048

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.