MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SCG Chemicals P350F Polypropylene copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: SCG PP P350F is a polypropylene copolymer without slip and anti-blocking agent designed suitable for cast film process with good seal properties, excellent clarity and good stress whitening resistance.

Applications: CPP retort film and general CPP film. Food and non-food packaging.

Applications produced by cast film process.

Features: Good seal properties. Excellent clarity. Good stress whitening resistance.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D 1505
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 620 %ASTM D882
Film Elongation at Break, TD 620 %ASTM D882
Flexural Modulus 800 MPaMD/TD; ASTM D790
2% Secant Modulus 330 MPaTD; ASTM D882
 350 MPaMD; ASTM D882
Izod Impact, Notched 3000 J/m
@Temperature 23.0 °C
ASTM D256
Film Tensile Strength at Break, MD 30.0 MPaASTM D882
Film Tensile Strength at Break, TD 8.00 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 161 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 10 %ASTM D1003
 
Descriptive Properties
AppearancePellet
Seal Strength>2 kgf/15mmBefore retort condition
 >2 kgf/15mmAfter retort condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC765 / 278022

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.