MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANRESIN® H 22 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DANRESIN® H 22 is an UV stable adhesive resin for PUR-, neoprene- and nitrile rubber-adhesives. DANRESIN® H 22 serves as an adhesive additive resin for the processing of contact adhesives. Because of the addition of DANRESIN® H 22 in adhesives the adhesion with rubber materials will be increased, the reactive temperature by PUR adhesives will be lowered and the "open time" of several adhesions will be prolonged.

Application: DANRESIN® H 22 is applied by the processing of adhesives which are used as adhesives in the field of maintenance, industrial branches and households were adhesives with non reactive or with low reactive temperatures during the appliances needed. Because of the very good ability to improve the adhesive characteristics DANRESIN® H 22 can also be applied for the modification of one-side adhesives. Adhesives modified and cross linked with isocyanates DANRESIN® H 22 are able to reach temperatures up to 120 °C.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccDIN 51.757
Solids Content 100 %DIN 53.189
Brookfield Viscosity 30 - 50 cPRVT
Storage Temperature 0.000 - 50.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CKofler
Softening Point 120 °CKofler
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectyellow - orange broken-resin
TypePolyurethane modified Alkyl- phenol resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ130 / 294550

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.