MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering Z95X Hydrogenated NBR Compound
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.

Applications: Gas blister resistant compound designed for use in applications where explosive decompression may occur. Suitable for use with sour (H2S) crude oil and gas, which may also include lubricating, oil additives and amine corrosion inhibitors. High mechanical strength and excellent chemical resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89°IRHD; ASTM D1415
 91°IRHD, +2 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 32.1 MPaASTM D412
 33.22 MPa3.5% change after 70 hours @ 150°C; ASTM D412
Elongation at Break 264 %ASTM D412
 273.24 %3.5% change after 70 hours @ 150°C; ASTM D412
Compression Set 20 %
@Temperature 150 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -25.0 °C
 -25.0 °CNon-brittle after 3 minutes
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering Z85L Hydrogenated NBR Compound
Precision Polymer Engineering V95X Fluoroelastomer Compound
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer
Precision Polymer Engineering N90M Nitrile Rubber
Precision Polymer Engineering Z95Z Hydrogenated NBR Compound

PPRECI162 / 57886

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.