MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F149 1581 Vacuum, Glass Reinforcement, Polyester Resin System
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Description: HexPly® F149 is a structural and electrical grade polyester resin system. It is self-extinguishing and exhibits high laminate strengths. HexPly® F149 can be tailored to any tack and drape, and cures at relatively low temperatures and pressures. It is a good oven cure type prepreg.

Benefits and Features

  • 250°F (121°C) Cure
  • Vacuum Bag, Autoclave, or Press Cure
  • Service Temperature up to 300°F (149°C)
  • Meets Requirements of MIL-R-7575C, Grades A and B, Class 0 and 4

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 70.0
Tensile Strength 50.0 ksiWet
 52.0 ksiDry
Tensile Modulus 3100 ksiWet
 3200 ksiDry
Flexural Strength 68.0 ksiWet
 70.0 ksiDry
Flexural Modulus 3200 ksiWet
 3300 ksiDry
Compressive Strength 48.0 ksiWet
 52.0 ksiDry
Compressive Modulus 3300 ksiWet
 3400 ksiDry
Shear Strength 3.10 ksiShort Beam, Wet
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.25
@Frequency 8.50e+9 - 1.00e+10 Hz
Dry
 4.33
@Frequency 8.50e+9 - 1.00e+10 Hz
Wet
Dielectric Loss Index 0.0110
@Frequency 8.50e+9 - 1.00e+10 Hz
Dry
 0.0150
@Frequency 8.50e+9 - 1.00e+10 Hz
Wet
 
Processing PropertiesOriginal ValueComments
Shelf Life 1.00 Month
@Temperature 21.0 °C
 3.00 Month
@Temperature 4.00 °C
 6.00 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9189 / 322345

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.