MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excellent room temperature formability and impart superior hot strength and high temperature oxidation resistance when compared to Type 409, Type 439, Type 430, 11 Cr-Cb™ and Type 436. This grade’s alloying additions, combined with AK Steel’s proprietary ULTRA FORM® processing technology, yield a fine, equiaxed grain structure that enhances room temperature formability and minimizes ridging.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 78 - 85Annealed
Tensile Strength, Ultimate 68.0 - 78.0 ksiAnnealed
 30.0 MPa
@Temperature 899 °C
0.059" Coil
 46.0 MPa
@Temperature 816 °C
0.059" Coil
 146 MPa
@Temperature 704 °C
0.059" Coil
 359 MPa
@Temperature 593 °C
0.059" Coil
Tensile Strength, Yield 45.0 - 55.0 ksi
@Strain 0.2 %
Annealed
 22.0 MPa
@Strain 0.2 %,
Temperature 899 °C
0.059" Coil
 39.0 MPa
@Strain 0.2 %,
Temperature 816 °C
0.059" Coil
 110 MPa
@Strain 0.2 %,
Temperature 704 °C
0.059" Coil
 164 MPa
@Strain 0.2 %,
Temperature 593 °C
0.059" Coil
Elongation at Break 28 - 37 %in 2 inches, Annealed
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 14.50 %
Iron, Fe 82.251 %Balance
Manganese, Mn 1.0 %
Nickel, Ni 0.30 %
Niobium, Nb (Columbium, Cb) 0.35 %
Nitrogen, N 0.011 %
Phosphorus, P 0.025 %
Silicon, Si 1.3 %
Sulfur, S 0.0030 %
Titanium, Ti 0.25 %
 
Descriptive Properties
Delta r0.5Annealed
r-bar1.3-1.6Annealed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work
Latrobe 440™ N-DUR High Quality Martensitic Stainless Steel
309 Stainless Steel, annealed, sheet
309 Stainless Steel, annealed, bar
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H1025

NAKS088a / 139268

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.