MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Cookson Group STAYSTIK® 472 Non-Filed Dielectric Interposer Film  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic

Material Notes: This thermoplastic adhesive film is designed for use in a variety of electronic applications. It is characterized by its excellent bonding at low process temperatures and extremely low ELASTIC MODULUS (60,000psi). The compliancy of this adhesive allows for the bonding of two materials having large dissimilarities in thermal expansion coefficients. The reworkability of this thermoplastic adhesive system offers many advantages in applications traditionally ill-suited to thermoset adhesives.

  • Fully polymerized resin - No "cure"
  • Easily reworkable - No outgassing
  • Bonds in seconds - Not hours or minutes
  • Low modulus reduces stress to bonded materials

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity >= 60.0 ksi
Adhesive Bond Strength >= 2000 psiDie shear adhesion, at 25°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+9 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.250 W/m-K
Maximum Service Temperature, Air 150 °CContinuous use
 <= 280 °CExcursion Temperature
Minimum Service Temperature, Air -65.0 °CContinuous use
Glass Transition Temp, Tg >= 25.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Monthat 25°C
 
Descriptive Properties
Attach Temperature125-200°C
Filler MaterialNone

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® PVDF Fluoropolymer Film
Overview of materials for Polyester Film
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge

PPLASK039 / 56329

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.