MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Plexus Plexus™ 3940 Methacrylate Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.

Fast tacking, low pressure sprayable adhesive with long bonding range, listed under UL INC.® Component recognition category MAGW2 (Adhesives, Isulation), File Number MH6288(N).

The solids weight is approximately 35%. The flash point is less than -20°F/less than -29°C. The color is clear/translucent, the consistency is medium liquid, and the application method is spray. The bond range holds up to 60 minutes. Peel strength is 23 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate.

Information provided by 3M Adhesives Division.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccUncured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 16.0 MPaASTM D638
Elongation at Break 150 %ASTM D638
Modulus of Elasticity 0.100 GPaASTM D638
Adhesive Bond Strength 12.0 MPaLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM914 / 53346

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.